Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of BERGAMID® A70C20 - PA66-CF20 - Avient Corporation

Material Data Center offers the following functions for BERGAMID® A70C20:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Bergamid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Resistant. Negligible, reversible or no changes in mass and dimensions.

Please consider the information about the application of the materials.
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 11000 / 16000 MPa ISO 527
断裂应力 150 / 220 MPa ISO 527
断裂伸长率 6 / 3 % ISO 527
简支梁冲击强度, +23°C 65 / 55 kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C - / 45 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 15 / 12 kJ/m² ISO 179/1eA
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 261 / * °C ISO 11357-1/-3
热变形温度, 1.80 MPa 245 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 250 / * °C ISO 75-1/-2
线性热膨胀系数, 平行 20 / * E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 70 / * E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 1.6 / * mm -
厚度为h时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 0.8 / * mm -
其它性能干 / 已调节单位Test Standard
吸水性 6.8 / * % 类似ISO 62
吸湿性 2.2 / * % 类似ISO 62
密度 - / 1220 kg/m³ ISO 1183
模塑测量的特殊性能干 / 已调节单位Test Standard
ISO数据
粘数. 150 / * cm³/g ISO 307, 1157, 1628
试样制备条件价值单位Test Standard
ISO数据
注塑, 熔体温度 280 °C ISO 294
注塑, 模具温度 80 °C ISO 294
典型数据
加工方法
注塑
供货形式
粒料
特殊性能
提高导电性, 防静电的
地区供应
欧洲
其他信息
注塑
Resistant. Negligible, reversible or no changes in mass and dimensions.

Please consider the information about the application of the materials.
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.